Phosphorous copper grades

Company standard
EN
PCU2
CW020A
PCU3
CW021A
PCU4
CW023A
Copper content
Cu + Ag + P
> 99,98 % > 99,98 % > 99,90 %
Phosphorus content 10 - 30 ppm 20 - 50 ppm 50 - 130 ppm
Electrical conductivity > 100 % IACS** > 98,28 % IACS** 90,5-96,9 % IACS**
other characteristics Resistant to
hydrogen embrittlement.

Good weldability and solderability.
Resistant to
hydrogen embrittlement.

In comparison with PCU2 improved
weldability and solderability.
Resistant to
hydrogen embrittlement.

Very good weldability and solderability.
Field of uses Electrical engineering, electronics, collector segments, cladding materials Applications in
electrical engineering for squarewave generators and switchgear devices
Apparatus
engineering

** The specification of electrical conductivity relates to the annealed condition